Now I've done a bit of testing, I'm a lot happier and more comfortable with what I've got to do. The test rectangles showed there was a small improvement with rounding the edges so I decided to do that.
.
I degreased as before with the caustic pumice paste and then sandblasted the ellipses in the blast cabinet:
.
Comparing the surface qualities of the non-blasted (left-hand side) with the blasted (right-hand side):
.
The plaques were blasted with compressed air, washed with a scrubbing brush and then placed into the sonic cleaner for good measure

for 5 minutes at 55°C
.
If there's any dust particles left on the plaque after all that then there is no justice!
I dried off the steel with a heat gun to dry it fast and avoid any rusting
.
That leaves me with eight sandblasted plaques ready to enamel
.
I sorted out the slightly rusty plaque to the left by re-sandblasting it. However, a bit of rust is not a problem for enamelling; the enamel itself becomes a strong acid when heated to fusing temperatures and can dissolve a bit of iron oxide. It's really the grease and oils that can hide inside the rust that are the problem. Anyway I got rid of it all the same!